Customization: | Available |
---|---|
Negative Materials: | All Suitable |
Cathode Materials: | Ncm Precursor Powder |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Model: T-NCM-O2
Package: 20g/bag
The cathode material of lithium cobalt oxide battery is lithium cobalt oxide LiCoO2, and the nickel cobalt manganese oxide battery is Li (NiCoMn) O2. It takes nickel salt, cobalt salt and manganese salt as raw materials. The proportion of nickel, cobalt and manganese can be adjusted according to actual needs. The safety of nickel cobalt manganese oxide battery is higher than that of lithium cobalt oxide battery. Both of them are good cathode materials, but their chemical properties are different. Therefore, their application fields are also different according to their different chemical properties.
NCMOH811 Lithium Nickel Cobalt Manganate High-nickel NCM811 Single Crystal Precursor Lithium Battery Cathode Material
NCM811 Precursor |
|
D10 (um) |
4.757 |
D50 (um) |
9.095 |
D90 (um) |
15.991 |
BET (m2/g) |
13.9071 |
Tap density (g/cm3) |
2.18 |
Capacity pergram(mAh/g) |
- |
Voltage (V) |
- |
Coin cell test condition |
- |
NCMOH622 Lithium Nickel Cobalt Manganate NCM622 Polycrystal Precursor Lithium Battery Cathode Material
NCM622 Precursor |
|
D10 (um) |
5.0 |
D50 (um) |
9.9 |
D90 (um) |
18.3 |
BET (m2/g) |
6.2 |
Tap density (g/cm3) |
2.27 |
NCMOH532 Lithium Nickel Cobalt Manganate NCM532 Polycrystal Precursor Lithium Battery Cathode Material
NCM523 Precursor |
|
D10 (um) |
5.9 |
D50 (um) |
10.4 |
D90 (um) |
17.9 |
BET (m2/g) |
7.1 |
Tap density (g/cm3) |
2.15 |