Separator Type: | / |
---|---|
Negative Materials: | / |
Electrolyte: | / |
Cathode Materials: | / |
Type: | Metallized Film, Foil |
Material: | Aluminum Laminated Film |
Customization: |
---|
Suppliers with verified business licenses
Layers from outside
(Shiny) to inside (Mat)
|
Polyamide (JIS Z1714): 0.025mm (+-0.0025mm) Adhesive (Polyester-polyurethane): 4-5 g/m2 Aluminum foil (JIS A8079,A8021): 0.040mm (+-0.004mm) Adhesive (Urethane-free Adhesive): 2-3 g/m2 Polypropylene: 0.040mm (+-0.004mm) |
Thickness
|
113μm
|
Width
|
400mm
|
Length
|
10m
|
Surface quality
|
Mat finish
|
Pinholes
|
Subject to the applicable aluminum foil standard
|
Impurity
|
1mm or less in diameter
|
Fish Eye
|
2mm or less in diameter (clear),1mm or less in diameter (colored)
|
Molding Depth
|
≥5.0mm
|
Electrical Insulating
|
Good
|
Hot Sealing Coniditon
|
180-190°C
|
Moisture Vapor / O2
Transmission Rate
|
200ppm / 5 years
|
Laminate Strength
|
Nylon/Al more than 2N/15mm Al/CPP more than 5N/15mm
|
Heat Seal Strength
|
More than 22.5N/15mm wide at 200ºC x 0.2Mpa x2 sec by TOB heat sealing
|
Solvent Retention
|
Less than 5mg/m2
|
Appearance
|
Within the sample of the limit
|
Slip Factor
|
CPP/CPP less than 1.0
|
Application Notes
|
Click the picture below to see the finished polymer Li-Ion battery made by heated sealer
|
Suppliers with verified business licenses