Customization: | Available |
---|---|
After-sales Service: | 1 Year |
Warranty: | 1year |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
SPECIFICATIONS
Project | Technical parameters | remarks |
Suitable system | Oil or water-based systems such as lithium iron phosphate, lithium cobalt oxide, lithium manganese oxide, lithium nickel cobalt oxide, lithium titanate, and graphite. |
|
Run substrate parameters | Aluminum foil(Cu): thickness 9-30um; Width 200-620mm Rolling diameter Max.500mm; Weight Max.500kg; Copper foil:(Cu): Thickness 6-30 um; Width 200-620mm; Rolling diameter Max.500mm; Weight Max.500kg; |
|
Design width of roller | 650mm | |
Ensure the coating width | 200-580mm | |
Mechanical running speed of equipment |
30m/min | |
Coating speed of equipment |
0.5-15m/min, machine checking<12m/min |
Depends on the drying condition |
Suitable slurry viscosity |
2000~16000 Cps(positive pole) 1000~16000 Cps(negtive pole) |
|
Single face coating thickness |
50~310g/m2 | |
Minimum intermittent length |
Coating speed less than 6m/min< 5mm; |
|
Minimum coating length for multiple sections |
20mm | Coating speed ≤10m/min |
Solvent character | Oily solvent NMP(s.g=1.033,b.p=204ºC); Aqueous solvent H2O/NMP(s.g=1.000,b.p=100ºC) |
|
Suitable solid content | Positive pole S.C. 60%±20%; Negative pole S.C. 50%±10%(PVDF system) S.C. 50%±5%(SBR system) |
|
proportion | Positive pole1.5-2.59/cm2; Negative pole 1~1.89/cm2 |
|
Coating mode | Double front and back 3 unequal interval transfer coating/ the second side automatically tracks/ continuous transfer coating |
|
Way of changing roll | Manual operation | |
Running direction of base material |
Forward coating, substrate positive and reverse empty foil running |